1. Draft angle and ejection direction

Cosmetic faces normally need 1–3 degrees of draft, and textured surfaces even more. Insufficient draft causes drag marks, ejector whitening and inconsistent cycle times. Parting line placement must be agreed together with appearance requirements.

2. Wall uniformity and ribs

Abrupt wall changes create sink marks and warpage. Rib thickness should stay around 50–60% of the nominal wall with generous root radii. Automotive interior parts and appliance housings benefit most from this review.

3. Gate location and runner system

The gate sets weld line position, packing efficiency and secondary finishing work. Hot runners suit high-volume multi-cavity tools, while cold runners fit frequent material changes and low-volume programs. The choice affects both tooling cost and unit price.

4. Resin grade and shrinkage

PP, PC+ABS and PA66+GF shrink very differently, and glass-filled grades add orientation-driven warpage. Flow analysis must use the approved grade rather than a generic family value.

5. Tolerances and inspection criteria

Define critical dimensions, tolerances and measurement method on the drawing, including CMM points, First Article Inspection items and cosmetic standards. After T0/T1 trials we submit dimensional reports and samples against that list.